Shanghai KaiYe latest products Inconel600 nickel-based corrosion resistant alloy

Inconel 600 alloy has the following features:

1. has good resistance to reduction, oxidation, corrosion performance nitride dielectric

2. At room temperature and high temperature have a very good resistance to stress corrosion cracking

3. has good resistance to dry chlorine and hydrogen chloride gas corrosion performance

4. When minus room temperature and high temperature have good mechanical properties

5. Has a good creep rupture strength, it is recommended for use in more than 700 ℃ work environment.

Inconel 600 metallurgical structure:

600 is a face-centered cubic lattice structure.

Inconel 600 corrosion resistance:
Alloy 600 for various corrosive media have corrosion resistance. Composition of the alloy of chromium under oxidising conditions than the nickel 99.2 (Alloy 200) and 99.2 Nickel (alloy 201, carbon) has better corrosion resistance. Meanwhile, the high nickel content of the alloy has good corrosion resistance in reducing conditions and alkaline solution, and can effectively prevent the chlorine - iron stress corrosion cracking. Alloy 600 has good corrosion resistance in acetic acid, acetic acid, formic acid, stearic acid and other organic acids, with moderate corrosion resistance in mineral acid. In a nuclear reactor primary and secondary high-purity water recycling has very good corrosion resistance. 600 In particular, outstanding performance is resistant to dry chlorine and hydrogen chloride corrosion, application temperature up to 650 ℃. At high temperatures, the alloy annealed and solution-treated condition has good antioxidant properties and high peeling strength in the air. The alloy is also resistant to ammonia and nitriding, carburizing atmosphere, but in alternate redox conditions, the alloy may be partially oxidized corrosive media (such as green death liquid)